Original language | English |
---|---|
Pages (from-to) | 1550022 |
Journal | International Journal of Computational Materials Science and Engineering |
Volume | 4 |
Issue number | 4 |
State | Published - 2015 |
Nanoindentation response of Fe-10%Cr bi-crystal structures with Σ5<001> and Σ3<110>tilt boundaries: An atomistic study
Mohammad Abu-Shams, Ishraq Shabib
Research output: Contribution to journal › Article › peer-review